| Nama merek: | DLX |
| Nomor Model: | Kawat Paduan FeCrAl 1Cr13Al4 |
| MOQ: | 10KG |
| Ketentuan Pembayaran: | L/C,D/A,D/P,T/T,Western Union |
| Kemampuan Pasokan: | 500 ton per bulan |
| 0Cr23Al5 | 0Cr21Al4 | 0Cr21Al6Nb | 0Cr27Al7Mo2 | Komposisi Kimia (%) - Cr | 12.0-15.0 | 23.0-26.0 | 19.0-22.0 |
|---|---|---|---|---|---|---|---|
| 20.5-23.5 | 18.0-21.0 | 21.0-23.0 | 26.5-27.8 | Komposisi Kimia (%) - Al | 4.0-6.0 | 4.5-6.5 | 5.0-7.0 |
| 4.2-5.3 | 3.0-4.2 | 5.0-7.0 | Sesuai | Komposisi Kimia (%) - Re | Sesuai | Sesuai | Sesuai |
| Sesuai | Sisa | Sisa | Sisa | Sisa | Sisa | Sisa | Sisa |
| Sisa | 1250 | 1250 | 1250 | 1250 | 1250 | 1250 | 1250 |
| 1250 | 1100 | Resistivitas pada 20°C (μΩ.m) | Resistivitas pada 20°C (μΩ.m) | Resistivitas pada 20°C (μΩ.m) | 1.25 | 1.42 | 1.42 |
| 1.35 | 1.23 | 1.53 | 1.53 | Kepadatan (g/cm³) | 7.4 | 7.1 | 7.16 |
| 7.25 | 7.35 | 63.2 | 7.1 | Konduktivitas Termal (KJ/m.h) | 52.7 | 63.2 | 63.2 |
| 60.2 | 46.9 | 16 | -- | Koefisien Ekspansi Linier (αx10⁻⁶/℃) | 15.4 | 16 | ≥80/1250 |
| 15 | 13.5 | 1500 | 16 | Titik Leleh Kira-kira (°C) | 1450 | 1500 | 1500 |
| 1500 | 1500 | 580-680 | 580-680 | 580-680 | 580-680 | 630-780 | 630-780 |
| 630-780 | 600-700 | Perpanjangan saat Putus (%) | Perpanjangan saat Putus (%) | Perpanjangan saat Putus (%) | >16 | >12 | >12 |
| >12 | >12 | 60-75 | 60-75 | 60-75 | 60-75 | 60-75 | 65-75 |
| 65-75 | >5 | 65-75 | >5 | >5 | >5 | >5 | >5 |
| >5 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 |
| 200-260 | ≥80/1300 | ≥80/1300 | ≥80/1300 | ≥80/1300 | ≥80/1300 | ≥80/1300 | ≥80/1300 |
| ≥80/1300 | ≥80/1250 | Struktur Mikrografis | Struktur Mikrografis | Struktur Mikrografis | Ferrit | Ferrit | Ferrit |
| Ferrit | Magnetik | Magnetik | Magnetik | Magnetik | Magnetik | Magnetik | Magnetik |
| Magnetik | Kawat | Kawat | Kawat | Kawat | Kawat | Kawat | Kawat |
| Batang | 8-50 |
|---|---|
| Pita | (0.05-0.35)×(0.5-6.0) |
| Strip | (0.5-2.5)×(5-180) |
| Fitur Utama Kawat Resistansi 1Cr13Al4 FeCrAl | Ketahanan Korosi Unggul |
| : Dirancang untuk menahan oksidasi dan korosi dalam elektrolit yang sangat basa atau asam, secara signifikan memperpanjang masa pakai sistem elektrolisis dan mengurangi biaya perawatan. | Stabilitas Suhu Tinggi |