| Kelas | Ni+Co | Cu | Ya. | Mn | C | Mg | S | P | Fe |
|---|---|---|---|---|---|---|---|---|---|
| N4 | 99.9 | ≤ 0.015 | ≤ 0.03 | ≤ 0.002 | ≤ 0.01 | ≤ 0.01 | ≤ 0.001 | ≤ 0.001 | ≤ 0.04 |
| N6 | 99.5 | 0.10 | 0.10 | 0.05 | 0.10 | 0.10 | 0.005 | 0.002 | 0.10 |
| Ni201 | ≥ 99.9 | ≤ 0.25 | ≤ 0.35 | ≤ 0.35 | ≤ 0.02 | / | ≤ 0.01 | / | ≤ 0.40 |
| Ni200 | ≥ 99.6 | ≤ 0.25 | ≤ 0.35 | ≤ 0.35 | ≤ 0.15 | / | ≤ 0.01 | / | ≤ 0.40 |
| Paduan | Ni+Co % | Mn % | Fe % | Si % | Cu % | C % | S % |
|---|---|---|---|---|---|---|---|
| Nikel 201 | 99 menit.2 | Max 0.35 | Max 0.4 | Max 0.35 | Max 0.25 | Max 0.02 | Max 0.01 |
| Nikel 200 | Min 99 | Max 0.35 | Max 0.4 | Max 0.35 | Max 0.25 | Max 0.15 | Max 0.01 |
| Kepadatan | Panas spesifik | Resistensi Listrik | Titik Peleburan | Konduktivitas Termal | Rata-rata Ekspansi Termal Coeff |
|---|---|---|---|---|---|
| 80,89 g/cm3 | 0.109 (456 J/kg°C) | 0.096*10−6 ohm.m | 1435-1446°C | 70.2 W/m-K | 13.3*10−6 m/m°C |